Method for smelting nickel oxide ore

Provided is a method for smelting nickel oxide ore by which the occurrence of cracking due to heat shock can be suppressed when nickel oxide ore is pelletized and charged into a smelting step (reduction step). A method for smelting nickel oxide ore according to the present invention uses pellets of...

Full description

Saved in:
Bibliographic Details
Main Authors Takahashi, Junichi, Inoue, Taku, Okada, Shuuji
Format Patent
LanguageEnglish
Published 07.08.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Provided is a method for smelting nickel oxide ore by which the occurrence of cracking due to heat shock can be suppressed when nickel oxide ore is pelletized and charged into a smelting step (reduction step). A method for smelting nickel oxide ore according to the present invention uses pellets of nickel oxide ore, the method being characterized by comprising a pellet production step S1 for producing pellets from nickel oxide ore, and a reduction step S2 for heating the resulting pellets at a predetermined reduction temperature in a reduction furnace, the reduction step S2 comprising preheating the pellets obtained in the pellet production step S1 to a temperature of 350 to 600° C. in the reduction furnace and thereafter charging the pellets into the reduction furnace and raising the temperature of the reduction furnace to the reduction temperature.
Bibliography:Application Number: US201515328634