Protective coating for metal surfaces

A method for heating or cooling a carbon containing reducing gas having a carbon monoxide content of at least 0.5 vol %, wherein the gas is heated to a temperature of at least 400° C. or wherein the gas is cooled from a temperature exceeding 400° C., wherein the gas is passed along a surface of a he...

Full description

Saved in:
Bibliographic Details
Main Authors Jeunink, Franciscus Arnoldus Maria, Risseeuw, Izaak Jacobus
Format Patent
LanguageEnglish
Published 07.08.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for heating or cooling a carbon containing reducing gas having a carbon monoxide content of at least 0.5 vol %, wherein the gas is heated to a temperature of at least 400° C. or wherein the gas is cooled from a temperature exceeding 400° C., wherein the gas is passed along a surface of a heating or cooling unit having a heat conductive metal or metal alloy body and a protective layer, which protective layer provides said surface, and which protective layer is made from a coating composition including colloidal amorphous silicate and crystalline oxide particles.
Bibliography:Application Number: US201314437104