METHOD FOR OBTAINING OF FUEL BRIQUETTES

A method for obtaining of fuel briquettes comprises the preparation of components, their mixing with binding agent, heating of mix and pressing. Into briquetting mix coal-tar pitch is supplied in quantity of 2-5 % of mass of raw material, mix is heated to the temperature of 310-320 ° , and pressing...

Full description

Saved in:
Bibliographic Details
Main Authors KYRYLCHENKO PETRO MYKOLAIOVYCH, OZHOHIN VOLODYMYR VOLODYMYROVYCH, NOSARIV OLEKSANDR ANDRIOVYCH, KOVALEVSKYI OLEKSII IHOREVYCH, SAVKOV ANATOLII OLEKSIOVYCH, FENTISOV IHOR MYKOLAIOVYCH, BOCHEK ANATOLII PAVLOVYCH, KLYMANCHUK VLADYSLAV VLADYSLAVOVYCH, CHERNOVA SVITLANA HENNADIIVNA
Format Patent
LanguageEnglish
Russian
Ukrainian
Published 10.10.2008
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for obtaining of fuel briquettes comprises the preparation of components, their mixing with binding agent, heating of mix and pressing. Into briquetting mix coal-tar pitch is supplied in quantity of 2-5 % of mass of raw material, mix is heated to the temperature of 310-320 ° , and pressing is carried out under pressure of 50-90 MPa. Способ получения топливных брикетов включает подготовку компонентов, смешивание их со связующим, нагрев смеси и прессование. В брикетируемую смесь вводят каменноугольный пек в количестве 2-5 % от массы сырья, нагревают смесь до температуры 310-320 °С, а прессование ведут под давлением 50-90 МПа. Спосіб одержання паливних брикетів включає підготовку компонентів, змішування їх із в'яжучим, нагрів суміші і пресування. В брикетовану суміш уводять кам'яновугільний пек у кількості 2-5 % від маси сировини, нагрівають суміш до температури 310-320 °С, а пресування ведуть під тиском 50-90 МПа.
Bibliography:Application Number: UA20080005618U