Process for reducing fogging from high melt strength polypropylene

Process for reducing fogging from high melt strength polypropylene (HMS-PP) obtained by heat treating polypropylene at a temperature between 150° C. and 300° C. in the presence of a dialkyl peroxydicarbonate, said process involving the introduction of an anhydride to said high melt strength polyprop...

Full description

Saved in:
Bibliographic Details
Main Authors FRIJLINK, WILHELM KLAAS, TALMA, AUKE GERARDUS, VAN DEN BERG, MICHEL, VAN DER SCHUUR, JAN MARTIJN
Format Patent
LanguageChinese
English
Published 01.01.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Process for reducing fogging from high melt strength polypropylene (HMS-PP) obtained by heat treating polypropylene at a temperature between 150° C. and 300° C. in the presence of a dialkyl peroxydicarbonate, said process involving the introduction of an anhydride to said high melt strength polypropylene.
Bibliography:Application Number: TW20165140333