Copper-beryllium alloy with high strength

A process for producing a copper-beryllium alloy product. The process comprises preparing a base alloy having 0.15 wt% - 4.0 wt% beryllium and having grains and an initial cross section area. The process further comprises cold working the base alloy to a percentage of cold reduction of area (CRA) gr...

Full description

Saved in:
Bibliographic Details
Main Authors TYSON, MICHAEL F, HOYER, JEFFREY S, GRENSING, FRITZ, ZIEGLER, KARL R, GATEHOUSE, JOHN E, SCHMECK, BRUCE D, GEDEON, MICHAEL J
Format Patent
LanguageChinese
English
Published 01.02.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process for producing a copper-beryllium alloy product. The process comprises preparing a base alloy having 0.15 wt% - 4.0 wt% beryllium and having grains and an initial cross section area. The process further comprises cold working the base alloy to a percentage of cold reduction of area (CRA) greater than 40%, based on the initial cross section area, and heat treating the cold worked alloy to produce the copper-beryllium alloy product. The grain structure of the copper-beryllium alloy product has an orientation angle of less than 45 DEG when viewed along the direction of the cold working. The copper-beryllium alloy product demonstrates a fatigue strength of at least 385 MPa after 106 cycles of testing.
Bibliography:Application Number: TW20209115349