Manufacturing process of composite sheet
To provide a manufacturing process which has not only moisture-permeable property and water resistance but also excellent heat resistance, weathering resistance and durability so as to be usable for industrial materials such as a waterproof sheet of housing, further does not volatilize a large amoun...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | Chinese English |
Published |
01.09.2008
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | To provide a manufacturing process which has not only moisture-permeable property and water resistance but also excellent heat resistance, weathering resistance and durability so as to be usable for industrial materials such as a waterproof sheet of housing, further does not volatilize a large amount of solvents such as a solvent type adhesive for use in a dry laminate, and less affects an environment when a composite sheet is manufactured by joining a hen the air-permeable reinforcement material is coated with a hot melt adhesive to adhere the olefine type porous film, the process comprises providing a roll first contact-bonding from the side of an olefine type porous film as a heating roll, setting the temperature of the heating roll in the range of from a temperature higher by 5 DEG C to a temperature lower by 15 DEG C than that of the extrapolated melting completion temperature of the olefine type porous film indicated by a differential scanning calorimetry, further setting the time for bringing the heati |
---|---|
Bibliography: | Application Number: TW20070141905 |