IMPROVED ALUMINIUM-COPPER-LITHIUM ALLOYS

FIELD: metallurgy.SUBSTANCE: method for manufacturing compres sed aluminium alloy product includes injection of aluminium alloy containing wt %: 3.4-4.2 Cu, 0.9-1.4 Li, 0.3-0.7 Ag, 0.1-0.6 Mg, 0.2-0.8 Zn, 0.1-0.6 Mn, the rest is aluminium and impurities, homogenization of aluminium alloy, pressing i...

Full description

Saved in:
Bibliographic Details
Main Authors KOGZUELL, Todd K, BREJ, Gari G, JOKUM, Les A, UILSON, Andre L, KOLVIN, Edvard L, DENTSER, Diana K, SOTELL, Ralf R, RIODZHA, Roberto Dzh
Format Patent
LanguageEnglish
Russian
Published 20.12.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: metallurgy.SUBSTANCE: method for manufacturing compres sed aluminium alloy product includes injection of aluminium alloy containing wt %: 3.4-4.2 Cu, 0.9-1.4 Li, 0.3-0.7 Ag, 0.1-0.6 Mg, 0.2-0.8 Zn, 0.1-0.6 Mn, the rest is aluminium and impurities, homogenization of aluminium alloy, pressing in pressed product, solid solution heat treatment, cold processing by 1-4% and artificial ageing.EFFECT: achieve improved combination of mechanical properties compared to alloys of known level of technology.28 cl, 2 ex, 8 tbl, 6 dwg Изобретение относится к алюминиево-медно-литиевым сплавам и может быть использовано в различных отраслях промышленности. Способ изготовления прессованного продукта из алюминиевого сплава включает литье алюминиевого сплава, содержащего, вес.%: 3,4-4,2 Cu, 0,9-1,4 Li, 0,3-0,7 Ag, 0,1-0,6 Mg, 0,2-0,8 Zn, 0,1-0,6 Mn, остальное - алюминий и примеси, гомогенизацию алюминиевого сплава, прессование в прессованный продукт, термообработку на твердый раствор, холодную обработку на 1-4% и искусственное старение. Изобретение направлено на достижение улучшенного сочетания механических свойств по сравнению со сплавами известного уровня техники. 27 з.п. ф-лы, 2 пр., 8 табл., 6 ил.