METHOD OF PRODUCTION OF STEEL POWDER WITH LOW OXYGEN CONTENT

FIELD: metallurgy.SUBSTANCE: method involves heat treatment of the steel powder at a temperature of 900-1200°C in a hydrogen medium and cooling in an argon medium. Prior to heat treatment of steel powder at a temperature of 900-1200°C the steel powder is heated up to a temperature of 600-750°C in ar...

Full description

Saved in:
Bibliographic Details
Main Authors Tokareva Olesya Vladimirovna, Arzhatkina Oksana Alekseevna, Kovaleva Irina Vladimirovna
Format Patent
LanguageEnglish
Russian
Published 11.07.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: metallurgy.SUBSTANCE: method involves heat treatment of the steel powder at a temperature of 900-1200°C in a hydrogen medium and cooling in an argon medium. Prior to heat treatment of steel powder at a temperature of 900-1200°C the steel powder is heated up to a temperature of 600-750°C in argon medium and held in carbon tetrachloride medium at a temperature of 600-750°C for 10-30 minutes. The heat treatment of the steel powder is carried out at a temperature of 900-1200°C in hydrogen medium for 40-60 minutes.EFFECT: reduction of labour intensity and duration of the powder production process.4 ex Изобретение относится к получению стального порошка с пониженным содержанием кислорода. Способ включает термообработку стального порошка при температуре 900-1200°С в среде водорода и охлаждение в среде аргона. Перед термообработкой стального порошка при температуре 900-1200°С проводят нагрев стального порошка до температуры 600-750°С в среде аргона и выдержку в среде четыреххлористого углерода при температуре 600-750°С в течение 10-30 минут. Термообработку стального порошка ведут при температуре 900-1200°С в среде водорода в течение 40-60 минут. Обеспечивается снижение трудоемкости и сокращение продолжительности процесса получения порошка. 4 пр.
Bibliography:Application Number: RU20150153097