ANTIPENETRATION WASH FOR CASTING MOULDS AND RODS

FIELD: metallurgy. ^ SUBSTANCE: antipenetration wash contains activated or milled or oxidated or extended cryptocrystalline graphite with ash content 2-13% and particle size 2-20 micrometre (29-56 wt %), binding agent (1.7-3.3 wt %), bentonite (5.0-9.3 wt %) and water (the rest). ^ EFFECT: there are...

Full description

Saved in:
Bibliographic Details
Main Authors NOVOZHONOV VLADIMIR IVANOVICH, BARANOV VLADIMIR NIKOLAEVICH, GIL'MANSHINA TAT'JANA RENATOVNA, MAMINA LJUDMILA IVANOVNA, BEZRUKIKH ALEKSANDR INNOKENT'EVICH
Format Patent
LanguageEnglish
Russian
Published 27.09.2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: metallurgy. ^ SUBSTANCE: antipenetration wash contains activated or milled or oxidated or extended cryptocrystalline graphite with ash content 2-13% and particle size 2-20 micrometre (29-56 wt %), binding agent (1.7-3.3 wt %), bentonite (5.0-9.3 wt %) and water (the rest). ^ EFFECT: there are increased processing characteristics of coating and it is reduced consumption of dry components. ^ 1 tbl Изобретение относится к литейному производству, в частности к составам противопригарных покрытий для литейных форм и стержней. Противопригарное покрытие содержит активированный, или обогащенный, или окисленный, или расширенный скрытокристаллический графит с зольностью 2-13% и размером частиц 2-20 мкм (29-56 мас.%), связующее (1,7-3,3 мас.%), бентонит (5,0-9,3 мас.%) и воду (остальное). Повышаются технологические свойства покрытия и сокращается расход сухих компонентов. 1 табл.
Bibliography:Application Number: RU20070149203