BAR ROLLING METHOD

FIELD: rolled stock production, possibly hot rolling of round bars of low alloy steel for cold die forging of fastening members. ^ SUBSTANCE: method comprises steps of heating blank up to 1100 - 1280°C; multi-pass hot rolling at reducing in grooved rolls at temperature of rolling process termination...

Full description

Saved in:
Bibliographic Details
Main Authors KHOREV GENNADIJ ALEKSANDROVICH, KRASNOV VLADIMIR VALENTINOVICH, TRAJNO ALEKSANDR IVANOVICH, MONID VLADIMIR ANATOL'EVICH, LUTSENKO ANDREJ NIKOLAEVICH
Format Patent
LanguageEnglish
Russian
Published 10.01.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: rolled stock production, possibly hot rolling of round bars of low alloy steel for cold die forging of fastening members. ^ SUBSTANCE: method comprises steps of heating blank up to 1100 - 1280°C; multi-pass hot rolling at reducing in grooved rolls at temperature of rolling process termination in range 950 - 1100°C; water cooling of rolled piece till 850 - 950°C. For rolled blank multi-pass rolling is realized at total elongation degree no less than 16. For cast billet multi-pass rolling is realized at total elongation degree no less than 36. Rolled bars are of alloy steel containing, mass %: carbon, 0.20 - 0.33; silicon, 0.17 - 035; manganese, 0.9 - 1.3; boron, 0.001 - 0.005; aluminum, 0.01 - 0.05; titanium, 0.01 or more; phosphorus, 0.035 of less; sulfur, 0.035 or less; chrome, 0.25 or less; nickel, 0.30 or less; copper, 0.30 or less; nitrogen, 0.012 or less; iron, the balance. ^ EFFECT: less loss of yield, improved quality of rolled bars. ^ 2 cl, 3 tbl, 2 ex
Bibliography:Application Number: RU20050119789