METHOD OF PREPARING SOLUTION FOR LEAD SALT PRODUCTION

FIELD: nonferrous metallurgy. SUBSTANCE: method comprises precipitate of lead salt at pH <1.5 from salt solution following etching of lead concentrate. Then, lead sulfate carbonization is carried out with (Na2CO3+CO2) solution at 50-60 C to form lead carbonate, which is dissolved in inorganic or...

Full description

Saved in:
Bibliographic Details
Main Authors KHOLMOGOROV A.G, PASHKOV G.L, MIKHLINA E.V, ZORINA N.V
Format Patent
LanguageEnglish
Russian
Published 10.10.2003
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: nonferrous metallurgy. SUBSTANCE: method comprises precipitate of lead salt at pH <1.5 from salt solution following etching of lead concentrate. Then, lead sulfate carbonization is carried out with (Na2CO3+CO2) solution at 50-60 C to form lead carbonate, which is dissolved in inorganic or organic solvent. EFFECT: avoided pyrometallurgic processes, increased lead recovery, and improved environmental safety. 1 dwg, 2 tbl, 3 ex
Bibliography:Application Number: RU20010132522