MEMBRANE DIFFUSEUR AUDIO AVEC CALLOTE ET PROCEDE DE REALISATION

The process comprises coating on both sides, of 100 per cent cotton linen weave, with identical warp and weft thicknesses, with styrene-butadiene-carboxylate latex (30-35 per cent). A 20-30 % polyurethane resin unilateral coating is also applied. Foularding at 20-25 deg C for 10 secs., drying at 135...

Full description

Saved in:
Bibliographic Details
Main Authors PREDESCU PAUL,RO, CUTIERU NATALIA,RO
Format Patent
LanguageFrench
Romanian
Published 28.02.1989
Edition4
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The process comprises coating on both sides, of 100 per cent cotton linen weave, with identical warp and weft thicknesses, with styrene-butadiene-carboxylate latex (30-35 per cent). A 20-30 % polyurethane resin unilateral coating is also applied. Foularding at 20-25 deg C for 10 secs., drying at 135-140 deg C, unilateral treatment with polyurethane resin, and repeat drying for forming over 2 mins at 6-6.5 kgf/cm2 and 145 deg C complete the work cycle.
Bibliography:Application Number: RO19860124895