METHODE DE PREPARATION DU MATERIAL ELECTRODIQUE ACTIF POUR L'ELECTRODE MEMBRANE CD2+ SELECTIF
The process active electrode comprises precipitation of a mixture of Cd(2+) and Ag(+) active electrode nitrates to form a CdS-Ag2S base. To obtain crystalline sulphides, the mixture is precipitated with the corresponding thioacetamide at CdS=Ag2S=1:1 to 4:1. The agitated process, at 2-5 degrees C, i...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | French Romanian |
Published |
30.09.1988
|
Edition | 4 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The process active electrode comprises precipitation of a mixture of Cd(2+) and Ag(+) active electrode nitrates to form a CdS-Ag2S base. To obtain crystalline sulphides, the mixture is precipitated with the corresponding thioacetamide at CdS=Ag2S=1:1 to 4:1. The agitated process, at 2-5 degrees C, is followed by heating for hours at 70-80 degrees C, and washing through repeated treatment with double-distilled water, first hot and then cold, filtration, washing with acetone, and vacuum drying at 40 degrees.C. |
---|---|
Bibliography: | Application Number: RO19860126168 |