PROCESS FOR PREPARING MASKING AND PROTECTIVE AGENTS FOR METALS TO BE SUBJECTED TO CHEMICAL WORKING
The invention relates to a process for preparing agents for masking and protecting metals subjected to chemical processing. According to the invention, the process consists in dissolving, in 8.5...8.6% tetra-chloro-ethylene, a mixture of 100 parts of styrene-butadiene star diblock-copolymer with a c...
Saved in:
Main Authors | , , , , , |
---|---|
Format | Patent |
Language | English Romanian |
Published |
30.05.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to a process for preparing agents for masking and protecting metals subjected to chemical processing. According to the invention, the process consists in dissolving, in 8.5...8.6% tetra-chloro-ethylene, a mixture of 100 parts of styrene-butadiene star diblock-copolymer with a content of 30.3% polystyrene having a molecular mass of 180000 g/mole and 50...60 parts, preferably 55 parts, of styrene-butadiene diblock-copolymer with a content of 70% polystyrene having a molecular mass of 80000 g/mole or 45...55 parts, preferably 50 parts, of styrene-butadiene diblock-copolymer with a content of 70% polystyrene having a molecular mass of 100000 g/mole.
Invenţia se referă la un procedeu pentru obţinerea unor agenţi de mascare şi protecţie a metalelor supuse uzinajului chimic. Procedeul conform invenţiei constă din dizolvarea în tetracloretilenă la o concentraţie de 8,5...8,6% a unui amestec format din 100 părţi dibloc-copolimer stiren-butadienic stelat cu un conţinut de 30,3% polistiren, având masa moleculară de 180.000 g/mol şi 50...60 părţi, preferabil 55 părţi dibloc-copolimer stiren-butadienic cu un conţinut de 70% polistiren, având masa moleculară de 80.000 g/mol sau 45...55 părţi, preferabil 50 părţi dibloc-copolimer stiren butadienic cu un conţinut de 70% polistiren, având masa moleculară de 100.000 g/mol. |
---|---|
Bibliography: | Application Number: RO20090000945 |