ELECTRODS PRODUCTION METHOD FOR WATER ACTIVATED BATTERYS
The process comprises heat treatment at 80-125 deg.C of CuCl2.2H2O with or without AgCl or PbCl2 treated at 100-150 deg.C for 4 hrs. and with temp. rise of 0.4-0.125 and 0.4-0.1 deg.C/min. respectively. Pouring into closed moulds for pressing, and coating of the prod. with a thin film by dipping in...