METHOD FOR SEQUESTRATION OF ARSENIC
There is provided a method and composition for sequestration of arsenic, the method comprising melting an arsenic-containing material in the presence of iron oxide and glass, and yielding a resulting glass incorporating arsenic. The resulting glass has an arsenic content comprised in a range between...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English Polish |
Published |
01.06.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | There is provided a method and composition for sequestration of arsenic, the method comprising melting an arsenic-containing material in the presence of iron oxide and glass, and yielding a resulting glass incorporating arsenic. The resulting glass has an arsenic content comprised in a range between 1 and 25% w/w and an iron content comprised in a range between 8 and 20% w/w. |
---|---|