AQUEOUS COATING MEDIUM, METHOD OF OBTAINING SAME AND APPLICATION THEREOF IN PRODUCTION OF STOVING LACQUERS AND OF COATING DRYING AS RESULT OF EXPOSURE TO PHYSICAL FACTORS

The use of an aqueous dispersion of a polyol component, comprising 20-60 wt.% unsaturated polyester polyol and 40-80 wt.% polyacrylate, and 1-70 wt.% (with respect to total solids) of a blocked aliphatic polyisocyanate component for light-stable, elastic, physically fast-drying coatings in series la...

Full description

Saved in:
Bibliographic Details
Main Authors IRLE CHRISTOPH, BLUM HARALD, PETZOLDT JOACHIM, MUELLER HEINO
Format Patent
LanguageEnglish
Polish
Published 30.11.2005
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The use of an aqueous dispersion of a polyol component, comprising 20-60 wt.% unsaturated polyester polyol and 40-80 wt.% polyacrylate, and 1-70 wt.% (with respect to total solids) of a blocked aliphatic polyisocyanate component for light-stable, elastic, physically fast-drying coatings in series lacquering of cars is claimed. The use of an aqueous dispersion of (A) a polyol component and (B) a polyisocyanate component for light-stable, elastic, physically fast-drying coatings in series lacquering of cars is claimed. The polyol component comprises 20-60 wt.% polyester component (AI) with 10-60 wt.% units derived from 8-30 carbon (C) aliphatic (un)saturated monocarboxylic acid(s) and 0.4-5 wt.% units derived from 3-8 C alpha , beta -unsaturated mono- or dicarboxylic acid(s) or anhydride(s) capable of free radical polymerization and 40-80 wt.% polyacrylate component (AII). The polyisocyanate component (B) comprises blocked aliphatic polyisocyanate(s) and is used in an amount of 1-70 wt.% with respect to total solids in the dispersion.
Bibliography:Application Number: PL19990334913