Method of processing waste materials containing calcium fluoride

The method allows processing waste materials containing calcium fluoride. Unique characteristics: The sludge left after the production of calcium phosphates, containing at least 1 percent by weight of Na and 3 percent by weight of P2O5 in terms of dry matter, is calcined at the temperature of 700-90...

Full description

Saved in:
Bibliographic Details
Main Authors KOWALSKI ZYGMUNT, PASZEK ANDRZEJ, DRZYMALA ZYGMUNT, PIWOWARSKI MICHAL
Format Patent
LanguageEnglish
Polish
Published 28.04.2000
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The method allows processing waste materials containing calcium fluoride. Unique characteristics: The sludge left after the production of calcium phosphates, containing at least 1 percent by weight of Na and 3 percent by weight of P2O5 in terms of dry matter, is calcined at the temperature of 700-900 degrees C for 1-2 hours. The product with the granulation above 15 mm is returned to the calcination process.
Bibliography:Application Number: PL19950309933