NOVEL POLYETHYLENE COMPOSITIONS AND METHODS OF MAKING AND USING SAME

A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590? F. to about 645? F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/s...

Full description

Saved in:
Bibliographic Details
Main Authors YU, Youlu, INN, Yongwoo, SUKHADIA, Ashish M, YANG, Qing, CRUZ, Carlos A, BARR, Jared L., III, FISHER, William, BRIDENDOLPH, Bill, MCDANIEL, Max, RUTLEDGE-RYAL, Brandy, FREY, Kelly, TSO, Chung Ching, HERT, Daniel G
Format Patent
LanguageEnglish
Published 11.02.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590? F. to about 645? F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/side and a neck-in of less than about 3.0 in/side.
Bibliography:Application Number: MY2019PI05581