PROCESS FOR PREPARING POLY(TRIMETHYLENE TEREPHTHALATE) FIBER

The present invention relates to processes using poly(trimethylene terephthalate) filaments (2)/yarn. The poly(trimethylene terephthalate) has a number average molecular weight of at least about 26500 and a melt viscosity of at least about 350 Pascals at 250 degree C and 48.65 per second shear rate....

Full description

Saved in:
Bibliographic Details
Main Author JINGUNG CHANG
Format Patent
LanguageEnglish
Spanish
Published 01.09.2006
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The present invention relates to processes using poly(trimethylene terephthalate) filaments (2)/yarn. The poly(trimethylene terephthalate) has a number average molecular weight of at least about 26500 and a melt viscosity of at least about 350 Pascals at 250 degree C and 48.65 per second shear rate. The poly(trimethylene terephthalate) is spun into filaments (2) and the filaments (2) are converged into yarn. The filaments have a denier greater than 1 and the yarn has a denier greater than 210. La presente invencion se refiere a procesos que usan filamentos de poli(trimetilentereftalato) (2)/hilo. El poli(trimetilentereftalato) tiene un numero de peso molecular promedio de por lo menos aproximadamente 26,500 y una viscosidad de fundido de por lo menos aproximadamente 350 Pascales a 250 degree C y una velocidad cortante de 48.65 por segundo. El poli(trimetilentereftalato) se hila en filamentos (2) y los filamentos (2) se convergen en hilo. Los filamentos tienen un denier mayor de 1 y el hilo tiene un denier mayor de 210.
Bibliography:Application Number: MX2006PA07683