PROCEDE DE FABRICATION D'UNE SOUDURE PAR POINTS PAR RESISTANCE

This method comprises the steps of:- providing at least two zinc or zinc-alloy coated sheets of a steel (1),- measuring C1av(100), Si1av(100), Mn1av(100), Al1av(100), Cr1av(100), , then- calculating the factor CSI1 of steel (1): CSI1=C1av100+Si1av100/32+Mn1av100/14−Al1av100/48+Cr1av100/11 then,- per...

Full description

Saved in:
Bibliographic Details
Main Authors GHASSEMI-ARMAKI, Hassan, CHAKRABORTY, Anirban, CHALLA VENKATASURYA, Pavan, GIRINA, Olga, PANAHI, Damon, BENLATRECHE, Yacine, PIPARD, Jean-Marc, CREMEL, Sébastien
Format Patent
LanguageFrench
Published 13.10.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:This method comprises the steps of:- providing at least two zinc or zinc-alloy coated sheets of a steel (1),- measuring C1av(100), Si1av(100), Mn1av(100), Al1av(100), Cr1av(100), , then- calculating the factor CSI1 of steel (1): CSI1=C1av100+Si1av100/32+Mn1av100/14−Al1av100/48+Cr1av100/11 then,- performing resistance spot welding,- measuring the average number Crack1av of Liquid Metal Embrittlement,- providing a second zinc or zinc-alloy coated steel sheet (2), the composition of steel (2) being selected so as : CSI2<CSI1−Crack1av−2/20- performing resistance spot welding on the steel sheet (2) with said intensity I1.
Bibliography:Application Number: MA20180054413