SYSTEME ET PROCEDE DE MINAGE EN SOLUTION POUR TRAITER DES FORMATIONS CONTENANT DES HYDROCARBURES

L¿INVENTION CONCERNE DES PROCÉDÉS DE TRAITEMENT D¿UNE FORMATION CONTENANT DES HYDROCARBURES AVANT L'UTILISATION D'UN PROCÉDÉ DE TRAITEMENT THERMIQUE IN SITU POUR OBTENIR DES HYDROCARBURES À PARTIR DE LA FORMATION, LESDITS PROCÉDÉS CONSISTANT À INTRODUIRE UN PREMIER FLUIDE COMPRENANT DE LA...

Full description

Saved in:
Bibliographic Details
Main Authors SCHOELING, LANNY, GENE, VINEGAR, HAROLD, J, DE ROUFFIGNAC, ERIC, PIERRE
Format Patent
LanguageFrench
Published 03.11.2008
Edition7
Online AccessGet full text

Cover

Loading…
More Information
Summary:L¿INVENTION CONCERNE DES PROCÉDÉS DE TRAITEMENT D¿UNE FORMATION CONTENANT DES HYDROCARBURES AVANT L'UTILISATION D'UN PROCÉDÉ DE TRAITEMENT THERMIQUE IN SITU POUR OBTENIR DES HYDROCARBURES À PARTIR DE LA FORMATION, LESDITS PROCÉDÉS CONSISTANT À INTRODUIRE UN PREMIER FLUIDE COMPRENANT DE LA VAPEUR OU DE L¿EAU CHAUFFÉE DANS UNE PARTIE DE LA FORMATION, LEDIT PREMIER FLUIDE ÉTANT INITIALEMENT À UNE TEMPÉRATURE INFÉRIEURE À UNE TEMPÉRATURE DE DISSOCIATION DE LA NAHCOLITE DANS LA FORMATION, À EXTRAIRE UN SECOND FLUIDE DE CETTE PARTIE DE LA FORMATION, LEDIT SECOND FLUIDE COMPRENANT DE LA NAHCOLITE ; À TRANSFÉRER DE LA CHALEUR À PARTIR D¿UN OU DE PLUSIEURS DISPOSITIFS DE CHAUFFAGE VERS LA FORMATION AFIN DE LA CHAUFFER ; ET À EXTRAIRE DES FLUIDES HYDROCARBONÉS DE LA FORMATION. AU FUR ET À MESURE DE LA PROGRESSION DE L¿EXPLOITATION PAR DISSOLUTION, LA TEMPÉRATURE DU PREMIER FLUIDE PEUT ÊTRE AUGMENTÉE DE MANIÈRE À CE QUE LA TEMPÉRATURE DU PREMIER FLUIDE ATTEIGNANT LA NAHCOLITE SOIT INFÉRIEURE À LA TEMPÉRATURE DE DISSOCIATION ET À CE QUE LA TEMPÉRATURE DU PREMIER FLUIDE SOIT INFÉRIEURE À LA TEMPÉRATURE DE PYROLYSE DES HYDROCARBURES DE LA FORMATION. A system for heating a hydrocarbon containing formation includes a heater having an elongated ferromagnetic metal heater section. The heater is located in an opening in a formation. The heater section is configured to heat the hydrocarbon containing formation. The exposed ferromagnetic metal has a sulfidation rate that goes down with increasing temperature of the heater, when the heater is in a selected temperature range.
Bibliography:Application Number: MA20080030937