METHOD FOR PREPARING SELENIUM-ENRICHED MODIFIED BIOCHAR FOR CADMIUM ADSORPTION
Disclosed is a method for preparing selenium-enriched modified biochar for cadmium adsorption. Selenium-enriched rice husks are impregnated in a hydrochloric acid solution of CaCl2 for 20 to 24 h, and the impregnated selenium-enriched rice husks are dried, and then carbonized at a carbonization temp...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
15.04.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Disclosed is a method for preparing selenium-enriched modified biochar for cadmium adsorption. Selenium-enriched rice husks are impregnated in a hydrochloric acid solution of CaCl2 for 20 to 24 h, and the impregnated selenium-enriched rice husks are dried, and then carbonized at a carbonization temperature of 300°C to 700°C for 0.5 to 1.5 h. The selenium- enriched biochar prepared in the disclosure has a specific surface area of 31.79 m2/g. After modification, the selenium element in the biochar plays a special role in promoting the adsorption of Cd2+, and cooperates with other multiple mechanisms to improve the adsorption performance of heavy metal Cd2+ in wastewater, and an adsorption capacity for Cd2+ with a concentration of 100 mg/L is 51.7 mg/g. |
---|---|
Bibliography: | Application Number: LU20230506396 |