METHOD FOR MANUFACTURING MINI-SPANGLE GALVANIZED STEEL WITH AN EXCELLENT DETACHABILITY OF AGEING RESISTANCE

The method includes the steps of; (a) galvanizing the steel plate in galvanizing solution bath containing 0.006-0.06 wt% Pb; (b) making mini spangle by spraying dihydrogen ammonium phosphate with pH 4.5-5.5 before solidifying molten zinc on the steel plate. The treated steel shows below 0.65 Pm lumi...

Full description

Saved in:
Bibliographic Details
Main Authors SHIN, JUNG - CHOL, CHON, SUN - HO, YUN, JAE - WOONG, KIM, JONG - SANG
Format Patent
LanguageEnglish
Korean
Published 20.06.1996
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The method includes the steps of; (a) galvanizing the steel plate in galvanizing solution bath containing 0.006-0.06 wt% Pb; (b) making mini spangle by spraying dihydrogen ammonium phosphate with pH 4.5-5.5 before solidifying molten zinc on the steel plate. The treated steel shows below 0.65 Pm luminous intensity and above 120 gloss intensity, has good peeling resistance.
Bibliography:Application Number: KR19930028645