PROCESS FOR THE PRODUCTION OF HYDROTHERMAL WATERGLASSES
Sodium silicate solutions having an SiO2:Na2O weight ratio of 1.95 to 1.6:1 are prepared hydrothermally by reaction of sand, sodium hydroxide and water. The invention is characterised in that the sand is reacted in less than a stoichiometric amount compared with the 2:1 weight ratio of the batch and...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English Korean |
Published |
27.03.1993
|
Edition | 5 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Sodium silicate solutions having an SiO2:Na2O weight ratio of 1.95 to 1.6:1 are prepared hydrothermally by reaction of sand, sodium hydroxide and water. The invention is characterised in that the sand is reacted in less than a stoichiometric amount compared with the 2:1 weight ratio of the batch and at temperatures between 190 and 240 DEG C. |
---|---|