HEAT-RESISTANT IRON-CHROMIUM-ALUMINIUM ALLOY WITH LOW CHROMIUM VAPORIZATION RATE AND ELEVATED THERMAL STABILITY
An iron-chromium-aluminum alloy with improved heat resistance, low chromium vaporization rate and good processability, comprising (in % by mass), 2.0 to 4.5% Al, 12 to 25% Cr, 1.0 to 4% W, 0.25 to 2.0% Nb, 0.05 to 1.2% Si, 0.001 to 0.70% Mn, 0.001 to 0.030% C, 0.0001 to 0.05% Mg, 0.0001 to 0.03% Ca,...
Saved in:
Main Authors | , , , , , , |
---|---|
Format | Patent |
Language | English Korean |
Published |
24.04.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | An iron-chromium-aluminum alloy with improved heat resistance, low chromium vaporization rate and good processability, comprising (in % by mass), 2.0 to 4.5% Al, 12 to 25% Cr, 1.0 to 4% W, 0.25 to 2.0% Nb, 0.05 to 1.2% Si, 0.001 to 0.70% Mn, 0.001 to 0.030% C, 0.0001 to 0.05% Mg, 0.0001 to 0.03% Ca, 0.001 to 0.030% P, max. 0.03% N, max. 0.01% S, remainder iron and the usual melting-related impurities. |
---|---|
Bibliography: | Application Number: KR20137033765 |