PROCESS FOR PRODUCING BROADER MOLECULAR WEIGHT DISTRIBUTION POLYMERS WITH A REVERSE COMONOMER DISTRIBUTION AND LOW LEVELS OF LONG CHAIN BRANCHES
The present invention provides an ethylene polymer having a melt index from about 0.1 to about 100 g/10 min; a ratio of Mw/Mn from 3 to 6; a reverse comonomer distribution; less than about 0.05 long chain branches (LCB) per 1000 total carbon atoms; and less than 5% by weight of the polymer eluted be...
Saved in:
Main Authors | , , , , , , , , , |
---|---|
Format | Patent |
Language | English Korean |
Published |
21.09.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The present invention provides an ethylene polymer having a melt index from about 0.1 to about 100 g/10 min; a ratio of Mw/Mn from 3 to 6; a reverse comonomer distribution; less than about 0.05 long chain branches (LCB) per 1000 total carbon atoms; and less than 5% by weight of the polymer eluted below a temperature of 40°C in an ATREF test. |
---|---|