PLANT-MIX TYPE ADDITIVE COMPOSITION AND POROUS ASPHALT COMPOSITION USING THE SAME

The present invention relates to a plant-mix type modifier composition, including: 20-35 wt% of a linear high-molecular weight styrene-butadiene-styrene copolymer having a weight average molecular weight of 150,000-350,000 g/mol; 25-35 wt% of a linear low-molecular weight styrene-butadiene-styrene c...

Full description

Saved in:
Bibliographic Details
Main Authors JANG SUNG BAE, JANG YOUNG DOO
Format Patent
LanguageEnglish
Korean
Published 15.02.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The present invention relates to a plant-mix type modifier composition, including: 20-35 wt% of a linear high-molecular weight styrene-butadiene-styrene copolymer having a weight average molecular weight of 150,000-350,000 g/mol; 25-35 wt% of a linear low-molecular weight styrene-butadiene-styrene copolymer having a weight average molecular weight of 50,000-150,000 g/mol; 10-15 wt% of a linear hydrogenated styrene-butadiene-styrene copolymer; 20-25 wt% of high-aromatic oil; and 5-10 wt% of a hydrogenated aromatic petroleum resin or hydrogenated aromatic-alicyclic copolymerized petroleum resin. According to the present invention, it is possible to prevent degradation of a modifier caused by the molecular thermal polymerization due to the heating of a polymer during the process for preparing an asphalt modifier used for a plant-mix process. 본 발명은 중량 평균 분자량이 15만 ~ 35만 g/mol인 선형 고분자량 스타이렌-부타디엔-스타이렌 공중합체 20 ~ 35 중량%; 중량 평균 분자량이 5만 ~ 15만 g/mol인 선형 저분자량 스타이렌-부타디엔-스타이렌 공중합체 25 ~ 35 중량%; 선형 수소첨가 스타이렌-부타디엔-스타이렌 공중합체 10 ~ 15 중량%; 고방향족 오일 20 ~ 25중량%; 수소첨가 방향족 석유수지 또는 수소첨가 방향족-지환족 공중합 석유수지 5 ~ 10중량%;를 포함하는 것을 특징으로 하는 플랜트 믹스 타입 개질재 조성물을 제시함으로써, 플랜트 믹스 방식에 사용되는 아스팔트 개질제의 제조 공정에서 고분자 폴리머의 가열에 의한 분자 열중합 반응에 따른 개질제 성능 저하를 방지할 수 있도록 한다.
Bibliography:Application Number: KR20210005434