FERRITE MAGNET, AND POWDER FOR FERRITE MAGNET AND PRODUCTION PROCESS THEREOF

PCT No. PCT/JP97/00962 Sec. 371 Date Oct. 3, 1997 Sec. 102(e) Date Oct. 3, 1997 PCT Filed Mar. 24, 1997 PCT Pub. No. WO97/35815 PCT Pub. Date Oct. 2, 1997It is an object of the present invention, in the W-type ferrite which is formulated as SrO.2(FeO).n(Fe2O3), to provide the ferrite magnet and the...

Full description

Saved in:
Bibliographic Details
Main Author TOYOTA, SACHIO
Format Patent
LanguageEnglish
Published 15.12.1999
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PCT No. PCT/JP97/00962 Sec. 371 Date Oct. 3, 1997 Sec. 102(e) Date Oct. 3, 1997 PCT Filed Mar. 24, 1997 PCT Pub. No. WO97/35815 PCT Pub. Date Oct. 2, 1997It is an object of the present invention, in the W-type ferrite which is formulated as SrO.2(FeO).n(Fe2O3), to provide the ferrite magnet and the manufacturing process thereof by which said W-type magnet maintains cost-performance characteristics recognized with the conventional M-type magnet and furthermore exhibits the maximum energy products more than 5 MGOe. In order to achieve the aforementioned object, carbon elements are admixed to raw powder which is a previously prepared mixture of SrCO3 and Fe2O3 under a given condition such that n-value in the above formula is in a range between 7.2 and 7.7. After the calcining said mixture, CaO, SiO2 and C powders are furthermore mixed and pulverized to have an average particle size of less than 0.06 mu m, followed by forming into a green compact body under a magnetic field and sintering the formed product under a non-oxidizing atmosphere. Hence the W-type ferrite, which has not been realized before, can be produced easily and with low cost.
Bibliography:Application Number: KR19970707699