MANUFACTURE OF HOT-AUSFORGED PRODUCT BY USING TOUGH AND HARD BORON STEEL
PURPOSE:To manufacture the titled product remarkably reduced in steel stock cost, by subjecting a hot-rolled steel stock containing specific percentages of C, Si, Mn, Cr, Cu, Sol Al, Ti, Nb, and B to heating, forging, and hardening under specific conditions. CONSTITUTION:A hot-rolled steel stock whi...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
11.11.1988
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PURPOSE:To manufacture the titled product remarkably reduced in steel stock cost, by subjecting a hot-rolled steel stock containing specific percentages of C, Si, Mn, Cr, Cu, Sol Al, Ti, Nb, and B to heating, forging, and hardening under specific conditions. CONSTITUTION:A hot-rolled steel stock which has a composition consisting of, by weight, 0.20-0.27% C, <=0.15% Si, 1.80-2.80% Mn, 0.25-0.50% Cr, <=0.13% Cu, 0.005-0.015% SolAl, 0.010-0.030% Ti, 0.020-0.050% Nb, 0.0020-0.0050% B, and the balance essentially iron with inevitable impurities is heated up to 1,000-1,300 deg.C. Subsequently, this steel stock is forged and then subjected to ausforging at >=950 deg.C (preferably 950-1,050 deg.C) in a cooling water of arbitrary temp. By this method, a hot-ausforged product of tough and hard boron steel having marked alloy-, energy-, and process-saving effects can be obtained. |
---|---|
Bibliography: | Application Number: JP19870108188 |