IMPACT MODIFIER FOR THERMOPLASTIC POLYOLEFIN RESIN

PROBLEM TO BE SOLVED: To obtain an impact modifier which is the most suitable for imparting impact resistance by mixing an ethylene/propylene random copolymer with a low-density or very low-density random copolymer of ethylene with an α-olefin having the specified number of carbon atoms in a specifi...

Full description

Saved in:
Bibliographic Details
Main Authors KAY PETER J, YU THOMAS C, OUHADI TRAZOLLAH
Format Patent
LanguageEnglish
Published 05.03.1999
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To obtain an impact modifier which is the most suitable for imparting impact resistance by mixing an ethylene/propylene random copolymer with a low-density or very low-density random copolymer of ethylene with an α-olefin having the specified number of carbon atoms in a specified ratio. SOLUTION: The ethylene/propylene random copolymer (A) used has a density of 0.850-0.900 g/cm and contains a nonconjugated diene containing 5-20 carbon atoms. The ethylene/4-20C α-olefin random copolymer (B) used has a density of 0.860-0.925 g/cm and a melt flow index of 0.2-30 dg/min and contains 5 wt.% 4-20C α-olefin (e.g. 1-butene) and a nonconjugated diene containing 5-20 carbon atoms. The mixing ratio A/B is (5-95) wt.%/(95-5 wt.%). The modifier is added in an amount of 4-60 wt.% based on a polypropylene composition containing selective additives.
Bibliography:Application Number: JP19980181479