PROBLEM TO BE SOLVED: To obtain a rough-surface film having an excellent rough surface and is excellent in resistances to impact and flex fatigue by preparing a rough- surface polyamide film with a surface unevenness having a specified central surface-average roughness and max. height. SOLUTION: A f...

Full description

Saved in:
Bibliographic Details
Main Authors IWANISHI MASUMI, IMAI KAZUMOTO, MORISHIGE CHIKAO, OKUMURA SHINICHIRO, MIKO TSUTOMU, SUGIMOTO MASANORI, MATSUDA AKIRA, OKUDAIRA HARUO
Format Patent
LanguageEnglish
Published 14.12.1999
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To obtain a rough-surface film having an excellent rough surface and is excellent in resistances to impact and flex fatigue by preparing a rough- surface polyamide film with a surface unevenness having a specified central surface-average roughness and max. height. SOLUTION: A film having at least one surface having a central surface- average roughness (SRa) of 0.05 μm or higher and a max. height (SRmax) of 1.40 μm or higher is prepd. Pref., such a film is prepd. by a method wherein a polyamide is mixed with an additive (e.g. an inorg. lubricant) and then formed into a film or wherein a mixture comprising at least two polymers including a polyamide is mixed with an inorg. lubricant and then formed into a film, and pref., the film is stretched. When a film having high strengths in addition to the above surface roughness in required, a laminated polyamide film is pref. which is prepd. by laminating the rough-surface polyamide film to at least one side of a polyamide film made of an aliph. polyamide.