To provide a bonded joint with excellent strength.SOLUTION: A bonded joint 1 comprises a steel section 10, an aluminum alloy section 20, and a diffusion layer 30 formed between the steel section 10 and the aluminum alloy section 20. The diffusion layer 30 is adjacent to the aluminum alloy section 20...

Full description

Saved in:
Bibliographic Details
Main Authors KADA OSAMU, MATSUI NAOKI, NARUMIYA HIROKI, SUZUKI ATSUSHI, ARAGAI YASUHARU
Format Patent
LanguageEnglish
Japanese
Published 07.05.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a bonded joint with excellent strength.SOLUTION: A bonded joint 1 comprises a steel section 10, an aluminum alloy section 20, and a diffusion layer 30 formed between the steel section 10 and the aluminum alloy section 20. The diffusion layer 30 is adjacent to the aluminum alloy section 20 and includes a diffusion region 32 adjacent to the aluminum alloy section with an Fe content ratio of 1.0 to 3.0% in the case where an Fe content in the steel section 10 is regarded as 100%. A thickness of the diffusion region 32 adjacent to the aluminum alloy section obtained by glow discharge optical emission spectrometry performed in a thickness direction of the diffusion layer 30 is 19.5 to 25.0 μm.SELECTED DRAWING: Figure 1 【課題】優れた強度を有する接合継手を提供する。【解決手段】本実施形態の接合継手1は、鋼部10と、アルミニウム合金部20と、鋼部10とアルミニウム合金部20との間に形成されている拡散層30とを備える。拡散層30は、アルミニウム合金部20と隣接し、鋼部10でのFe含有量を100%とした場合のFe含有量比率が1.0~3.0%であるアルミニウム合金部隣接拡散領域32を含み、拡散層30の厚さ方向にグロー放電発光分析を実施して得られたアルミニウム合金部隣接拡散領域32の厚さが19.5~25.0μmである。【選択図】図1
Bibliography:Application Number: JP20220168794