TERBIUM-CONTAINING PARAMAGNETIC GARNET-TYPE TRANSPARENT CERAMIC, AND MAGNETO-OPTICAL DEVICES

To provide a terbium-containing paramagnetic garnet-type transparent ceramic having low absorption at a wavelength of 1,064 nm and a temperature coefficient of refractive index that is half or less that of existing TGG crystals.SOLUTION: A sintered compact of a composite oxide comprises terbium, ytt...

Full description

Saved in:
Bibliographic Details
Main Authors TANAKA KEITA, MATSUMOTO TAKUSHI, IKARI MASANORI
Format Patent
LanguageEnglish
Japanese
Published 14.09.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a terbium-containing paramagnetic garnet-type transparent ceramic having low absorption at a wavelength of 1,064 nm and a temperature coefficient of refractive index that is half or less that of existing TGG crystals.SOLUTION: A sintered compact of a composite oxide comprises terbium, yttrium and aluminum, wherein: a volume molar concentration of terbium is equal to or more than the volume molar concentration of yttrium; the Verde constant at a wavelength of 1,064 nm is 30 rad/(T-m) or more; and the average value (dn(1064)/dt)ave of a temperature coefficient of refractive index at 1,064 nm and temperatures of 20, 30, and 40°C is equal to or less than 9.0×10-6(K-1).SELECTED DRAWING: Figure 1 【課題】波長1064nmで低吸収率であると共に、屈折率の温度係数が既存のTGG結晶の半分以下であるテルビウム含有常磁性ガーネット型透明セラミックスを提供する。【解決手段】テルビウムとイットリウムとアルミニウムとを含み、該テルビウムの含有体積モル濃度がイットリウムの含有体積モル濃度以上である複合酸化物の焼結体であり、波長1064nmにおけるベルデ定数が30rad/(T・m)以上であり、波長1064nm、温度20、30、40℃における屈折率の温度係数の平均値(dn(1064)/dt)aveが9.0×10-6(K-1)以下である。【選択図】図1
Bibliography:Application Number: JP20220032239