RESIN COMPOSITION

To provide a resin composition which contains a polyphenylene sulfide resin, is excellent in low warpage properties, heat resistance and flame retardancy, has less corrosiveness to metals, and is also excellent in mechanical strength and chemical resistance.SOLUTION: The resin composition contains 5...

Full description

Saved in:
Bibliographic Details
Main Authors MUTO FUMIHIRO, IZEKI SHUTA
Format Patent
LanguageEnglish
Japanese
Published 30.05.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a resin composition which contains a polyphenylene sulfide resin, is excellent in low warpage properties, heat resistance and flame retardancy, has less corrosiveness to metals, and is also excellent in mechanical strength and chemical resistance.SOLUTION: The resin composition contains 5-150 pts.mass of a fibrous filler (D) and 1-20 pts.mass of a bromine-based flame retardant (E) based on 100 pts.mass of the total of (A)-(C) containing: 25-65 pts.mass of a polyphenylene sulfide resin (A) having an MVR of 60-500 cm3/10 min; and 35-75 pts.mass of the total of amorphous rubber-reinforced polystyrene or polystyrene (B) and/or a polyphenylene ether resin (C).SELECTED DRAWING: None 【課題】ポリフェニレンスルフィド樹脂を含有し、低反り性、耐熱性及び難燃性に優れ、金属に対する腐食性が少なく、機械的強度や耐薬品性にも優れる樹脂組成物。【解決手段】MVRが60~500cm3/10minのポリフェニレンスルフィド樹脂(A)を25~65質量部、非晶性のゴム強化ポリスチレン若しくはポリスチレン(B)及び/又はポリフェニレンエーテル樹脂(C)を、(B)と(C)の合計で35~75質量部を含有する(A)~(C)の合計100質量部に対し、繊維状フィラー(D)を5~150質量部、臭素系難燃剤(E)を1~20質量部含有することを特徴とする樹脂組成物。【選択図】なし
Bibliography:Application Number: JP20220015652