SOLUTION: To provide an electrolyte that includes a polymeric material, a lithium salt, an organic solvent, a plasticizer, an ionic solution, and an auxiliary material, which are kneaded into a colloidal form, and in which the polymeric material is 20 to 45% by weight, the lithium salt is 2 to 10% b...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
25.05.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | SOLUTION: To provide an electrolyte that includes a polymeric material, a lithium salt, an organic solvent, a plasticizer, an ionic solution, and an auxiliary material, which are kneaded into a colloidal form, and in which the polymeric material is 20 to 45% by weight, the lithium salt is 2 to 10% by weight, the organic solvent is 10 to 20% by weight, the plasticizer is 10 to 20% by weight, the ionic solution is 1 to 4% by weight, the auxiliary material is 1 to 4% by weight, and a manufacturing method thereof.EFFECT: A colloidal electrolyte according to the present invention has low fluidity due to its high cohesive mechanical properties, and the ionic conductivity is also clearly improved over solid electrolytes, realizes properties such as high ionic conductivity, no need for spacers, and useful for adhesion to glass, plastic, and the like, and avoids liquid leakage due to high safety, and also has high adhesion, high light transmittance, and high conductivity.SELECTED DRAWING: Figure 1
【解決手段】本発明は電解質及びその製造方法を開示する。該電解質は、高分子材料と、リチウム塩と、有機溶媒と、可塑剤と、イオン性溶液と、補助材料と、を含み、これらを混練してコロイド状にしたものであり、該高分子材料は20~45重量%、該リチウム塩は2~10重量%、該有機溶媒は10~20重量%、該可塑剤は10~20重量%、該イオン性溶液は1~4重量%、該補助材料は1~4重量%である。【効果】本発明のコロイド電解質は、凝集機械的性質が高いため低流動性を有し、イオン伝導率も固体電解質よりも明らかに向上し、イオン伝導率が高い、スペーサを必要としない、ガラスやプラスチックなどの粘着に有用であるなどの特性を実現する。安全性が高いので液漏れを回避し、また、高粘着性、高透光率及び高伝導率を有する。【選択図】図1 |
---|---|
Bibliography: | Application Number: JP20220169631 |