POLISHING COMPOSITION, POLISHING METHOD AND SEMICONDUCTOR SUBSTRATE MANUFACTURING METHOD
To provide means for suppressing part of a polishing target from being left unpolished and the occurrence of dishing in polishing the target including polycrystalline silicon and silicon nitride.SOLUTION: A polishing composition comprises: abrasive grains; ammonia; and at least one potassium compoun...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
13.10.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | To provide means for suppressing part of a polishing target from being left unpolished and the occurrence of dishing in polishing the target including polycrystalline silicon and silicon nitride.SOLUTION: A polishing composition comprises: abrasive grains; ammonia; and at least one potassium compound selected from a group consisting of potassium hydroxide and a potassium salt. In the polishing composition, a content of the ammonia is 0.002 mass% or more and 0.5 mass% or less to a total mass of the polishing composition, and a content of the potassium compound is 0.004 mass% or more and 0.5 mass% or less to the total mass of the polishing composition.SELECTED DRAWING: None
【課題】ポリシリコンおよび窒化ケイ素を含む研磨対象物の研磨において、研磨残りおよびディッシングの両方を抑制できる手段を提供する。【解決手段】砥粒と、アンモニアと、水酸化カリウムおよびカリウム塩からなる群から選択される少なくとも1種のカリウム化合物とを含む研磨用組成物であって、前記アンモニアの含有量は前記研磨用組成物の総質量に対して0.002質量%以上0.5質量%以下であり、前記カリウム化合物の含有量は前記研磨用組成物の総質量に対して0.004質量%以上0.5質量%以下である、研磨用組成物。【選択図】なし |
---|---|
AbstractList | To provide means for suppressing part of a polishing target from being left unpolished and the occurrence of dishing in polishing the target including polycrystalline silicon and silicon nitride.SOLUTION: A polishing composition comprises: abrasive grains; ammonia; and at least one potassium compound selected from a group consisting of potassium hydroxide and a potassium salt. In the polishing composition, a content of the ammonia is 0.002 mass% or more and 0.5 mass% or less to a total mass of the polishing composition, and a content of the potassium compound is 0.004 mass% or more and 0.5 mass% or less to the total mass of the polishing composition.SELECTED DRAWING: None
【課題】ポリシリコンおよび窒化ケイ素を含む研磨対象物の研磨において、研磨残りおよびディッシングの両方を抑制できる手段を提供する。【解決手段】砥粒と、アンモニアと、水酸化カリウムおよびカリウム塩からなる群から選択される少なくとも1種のカリウム化合物とを含む研磨用組成物であって、前記アンモニアの含有量は前記研磨用組成物の総質量に対して0.002質量%以上0.5質量%以下であり、前記カリウム化合物の含有量は前記研磨用組成物の総質量に対して0.004質量%以上0.5質量%以下である、研磨用組成物。【選択図】なし |
Author | TADA MAKI YOSHIZAKI YUKINOBU NAGANO TAKAHITO IKAWA HIROFUMI MAE RYOTA |
Author_xml | – fullname: YOSHIZAKI YUKINOBU – fullname: IKAWA HIROFUMI – fullname: MAE RYOTA – fullname: TADA MAKI – fullname: NAGANO TAKAHITO |
BookMark | eNrjYmDJy89L5WSICPD38Qz28PRzV3D29w3wD_YM8fT301FACPu6hnj4uyg4-rkoBLv6ejr7-7mEOof4BykEhzoFhwQ5hrgq-Dr6hbo5OoeEBiE08DCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMjI0NTExNTE0djohQBAOhPNAo |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 研磨用組成物、研磨方法、および半導体基板の製造方法 |
ExternalDocumentID | JP2022154454A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_JP2022154454A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:59:12 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English Japanese |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_JP2022154454A3 |
Notes | Application Number: JP20210057504 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221013&DB=EPODOC&CC=JP&NR=2022154454A |
ParticipantIDs | epo_espacenet_JP2022154454A |
PublicationCentury | 2000 |
PublicationDate | 20221013 |
PublicationDateYYYYMMDD | 2022-10-13 |
PublicationDate_xml | – month: 10 year: 2022 text: 20221013 day: 13 |
PublicationDecade | 2020 |
PublicationYear | 2022 |
RelatedCompanies | FUJIMI INC |
RelatedCompanies_xml | – name: FUJIMI INC |
Score | 3.5589745 |
Snippet | To provide means for suppressing part of a polishing target from being left unpolished and the occurrence of dishing in polishing the target including... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ADHESIVES BASIC ELECTRIC ELEMENTS CHEMISTRY DRESSING OR CONDITIONING OF ABRADING SURFACES DYES ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ELECTRICITY FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS GRINDING MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS PAINTS PERFORMING OPERATIONS POLISHES POLISHING SEMICONDUCTOR DEVICES TRANSPORTING |
Title | POLISHING COMPOSITION, POLISHING METHOD AND SEMICONDUCTOR SUBSTRATE MANUFACTURING METHOD |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20221013&DB=EPODOC&locale=&CC=JP&NR=2022154454A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dS8Mw8JhT1DedynQqQaRPFtePrd3DkC5pmYM2ZWtlbyNNM1BhG67i3zepndvT3pIcOZKDu8td7gPgkTki57ZwdJ6rFmYua-ss61n6fJ6xnFvCFKKM8o26w9QeTTvTGnxucmHKOqE_ZXFEyVFc8ntRyuvV1olFytjK9XP2LpeWL0HSJ1plHZvSgDEsjQz6fkwJxRrG_VGsReM_mCo8Y3sHcCjf0Y6K__LfBiotZbWrU4IzOIolukVxDrUP1oATvGm91oDjsPrxlsOK-dYXMI1p5V5CmIYxnbwq99IT2i6HfjKkBHkRQRNFXxqRFCd0jCbpQDVHTnwUelEaeDhJx9sNl_AQ-Ake6vKIs3-CzEbxznWsK6gvlgvRBNR2mWl0e9Ji6GQ2N9zM6XBmZ3YvN3ObufwaWnsQ3eyFtuBUzZTYNqxbqBdf3-JO6uMiuy_p-AvaaIiA |
link.rule.ids | 230,309,783,888,25578,76884 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dT8Iw8IJoxDdFjYofizF7ctF9AOOBmNFuGcjWBTbDG-m6kqgJEJnx79vOITzx1tyll_aSu-td7wPggbZ5xize1lgmR5jZ9FmjacfUZrOUZszkBudFlm_Y8hNrMGlOKvC5roUp-oT-FM0RhUQxIe95oa-XmyAWLnIrV0_puwAtXry4i9XSOzaEA6ObKu513YhgglSEuoNIDUd_ONl4xnL2YF-8sW3ZaN9968mylOW2TfGO4SAS5Ob5CVQ-aB1qaD16rQ6HQfnjLZal8K1OYRKRMrykIBJEZNyX4aVHZQMO3NgnWHFCrIwlf0mIExSTkTJOenI4cuwqgRMmnoPiZLTZcAb3nhsjXxNHnP4zZDqItq5jnkN1vpjzC1CebWrorY7wGJqpxXQ7bTcZtVKrkxmZRW12CY0dhK52Yu-g5sfBcDrsh68NOJIYqcJ18xqq-dc3vxG2OU9vC57-AmoTi3A |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=POLISHING+COMPOSITION%2C+POLISHING+METHOD+AND+SEMICONDUCTOR+SUBSTRATE+MANUFACTURING+METHOD&rft.inventor=YOSHIZAKI+YUKINOBU&rft.inventor=IKAWA+HIROFUMI&rft.inventor=MAE+RYOTA&rft.inventor=TADA+MAKI&rft.inventor=NAGANO+TAKAHITO&rft.date=2022-10-13&rft.externalDBID=A&rft.externalDocID=JP2022154454A |