RADOME
To improve the quality of a radome which uses a cyanate ester resin for a skin layer.SOLUTION: A radome 10 is formed by a multilayer body, in which a plurality of skin layers is laminated on a surface of a core material 12. The plurality of skin layers includes a first fiber-reinforced plastic layer...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
26.07.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | To improve the quality of a radome which uses a cyanate ester resin for a skin layer.SOLUTION: A radome 10 is formed by a multilayer body, in which a plurality of skin layers is laminated on a surface of a core material 12. The plurality of skin layers includes a first fiber-reinforced plastic layer 20, which contains a cyanate ester resin and a fiber material, and a second fiber-reinforced plastic layer 16, which contains an epoxy resin and a fiber material. The second fiber-reinforced plastic layer 16 is arranged in a position where the skin layer is in contact with the surface of the core material 12. It is preferable that the proportion of the thickness of the second fiber-reinforced plastic layer 16 in the total thickness of the skin layer is 50% or less.SELECTED DRAWING: Figure 2
【課題】シアネートエステル樹脂をスキン層に用いたレドームの品質を向上する。【解決手段】レドーム10は、コア材12の表面に複数のスキン層を積層した積層体で形成されている。複数のスキン層は、シアネートエステル樹脂と繊維素材とを含有する第1の繊維強化プラスチック層20と、エポキシ樹脂と繊維素材とを含有する第2の繊維強化プラスチック層16とを備え、コア材12の表面と接する位置には、第2の繊維強化プラスチック層16が配置されている。第2の繊維強化プラスチック層16の厚さがスキン層全体の厚さに占める割合は50%以下であることが好ましい。【選択図】図2 |
---|---|
Bibliography: | Application Number: JP20210003624 |