SINTERED MATERIAL AND METHOD FOR MANUFACTURING SINTERED MATERIAL

To provide a sintered material reduced in weight and having low thermal expansion.SOLUTION: A sintered material contains 20-60 mass% of nickel, the balance being iron and inevitable impurities, and has a porosity of 25-60%. The pore size is preferably 50-200 μm. The density is preferably 4.0-6.0 g/m...

Full description

Saved in:
Bibliographic Details
Main Authors OGAWA TETSUYA, ISHIHARA CHIO, SHIOTANI MAYU, SUDA SOICHIRO, NAKAYAMA NORIYUKI
Format Patent
LanguageEnglish
Japanese
Published 11.03.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a sintered material reduced in weight and having low thermal expansion.SOLUTION: A sintered material contains 20-60 mass% of nickel, the balance being iron and inevitable impurities, and has a porosity of 25-60%. The pore size is preferably 50-200 μm. The density is preferably 4.0-6.0 g/m3.SELECTED DRAWING: Figure 1 【課題】軽量化された低熱膨張性の焼結材料を提供することができる。【解決手段】20〜60質量%のニッケルを含み、残部が鉄及び不可避不純物からなり、気孔率が25〜60%である、焼結材料である。好ましくは、気孔サイズが50〜200μmである。好ましくは、密度が4.0〜6.0g/m3である。【選択図】図1
Bibliography:Application Number: JP20190158351