OPAQUE RESIN BASE FOR PINBALL GAME AND ITS MANUFACTURING METHOD, AND RESIN BASE FOR PINBALL GAME WITH PRINT FILM

To provide a resin base for a pinball game in which the color rendering property of a print film is good even when the print film is laminated directly.SOLUTION: A resin base (10) for a pinball game of the present invention comprises a transparent thermoplastic resin composition layer containing a f...

Full description

Saved in:
Bibliographic Details
Main Authors OSAWA YUJI, SHIODA MICHITAKA, TAGA SHO
Format Patent
LanguageEnglish
Japanese
Published 08.10.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a resin base for a pinball game in which the color rendering property of a print film is good even when the print film is laminated directly.SOLUTION: A resin base (10) for a pinball game of the present invention comprises a transparent thermoplastic resin composition layer containing a first transparent thermoplastic resin (A) and a second transparent thermoplastic resin (B) different in the refraction index. The resin base (10) for the pinball game of the present invention has the thickness of 8-22 mm, and an absolute value of a difference between the refraction index (nA) of the first transparent thermoplastic resin (A) and the refraction index (nB) of the second transparent thermoplastic resin (B) is 0.01 or more. The thermoplastic resin composition layer has an overall light transmittance of 80% or less and a haze of 10% or more.SELECTED DRAWING: Figure 1 【課題】印刷フィルムを直接積層した場合にも印刷フィルムの演色性が良好な弾球遊技用樹脂基盤を提供する。【解決手段】本発明の弾球遊技用樹脂基盤(10)は、屈折率の異なる第1の透明熱可塑性樹脂(A)と第2の透明熱可塑性樹脂(B)とを含有する熱可塑性樹脂組成物層を含む。本発明の弾球遊技用樹脂基盤(10)は、厚みが8〜22mmであり、第1の透明熱可塑性樹脂(A)の屈折率(nA)と第2の透明熱可塑性樹脂(B)の屈折率(nB)との差の絶対値が0.01以上である。熱可塑性樹脂組成物層は、全光線透過率が80%以下かつヘイズが10%以上である。【選択図】図1
Bibliography:Application Number: JP20190065364