To provide a room temperature curable polyorganosiloxane composition which has excellent adhesion to various substrates and forms a cured product with an excellent elongation property.SOLUTION: A room temperature curable polyorganosiloxane composition contains: (A) 100 pts.mass of linear polyorganos...

Full description

Saved in:
Bibliographic Details
Main Authors OTASHIRO KOKI, ONO KAZUHISA
Format Patent
LanguageEnglish
Japanese
Published 20.02.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a room temperature curable polyorganosiloxane composition which has excellent adhesion to various substrates and forms a cured product with an excellent elongation property.SOLUTION: A room temperature curable polyorganosiloxane composition contains: (A) 100 pts.mass of linear polyorganosiloxanes having two or more alkoxy groups in each molecule; (B1) 1-100 pts.mass of mica powder; (B2) 3-50 pts.mass of aerosol silica; (C) 0.5-15 pts.mass of an alkoxysilane represented by general formula RSi(OR), or a partial hydrolysis condensate thereof, where Ris monovalent hydrocarbon group, Ris an alkyl group or alkoxy substituted alkyl group, and a is 0, 1 or 2; and (D) 0.1-10 pts.mass of a titanium chelate catalyst.SELECTED DRAWING: None 【課題】各種基材への接着性に優れ、また、硬化物に優れた伸び特性を与える室温硬化性ポリオルガノシロキサン組成物の提供。【解決手段】(A)一分子中に2つ以上のアルコキシ基を有する直鎖状のポリオルガノシロキサンの100質量部、(B1)マイカ粉末の1〜100質量部、(B2)煙霧質シリカの3〜50質量部、(C)一般式:R1aSi(OR2)4−a(式中、R1は1価炭化水素基、R2はアルキル基又はアルコキシ置換アルキル基、aは0、1、又は2である。)で表されるアルコキシシラン又はその部分加水分解縮合物の0.5〜15質量部、及び(D)チタンキレート触媒の0.1〜10質量部を含有する室温硬化性ポリオルガノシロキサン組成物。【選択図】なし
Bibliography:Application Number: JP20180152582