METHOD FOR PRODUCING FIBROUS CARBON NANO STRUCTURE DISPERSION

To provide a method for efficiently producing a fibrous carbon nano structure dispersion excellent in long-term stability while preventing the occurrence of bubbling during dispersion treatment.SOLUTION: A method for producing a fibrous carbon nano structure dispersion includes a step of subjecting...

Full description

Saved in:
Bibliographic Details
Main Authors YAMAGISHI TOMOKO, UEJIMA MITSUGI
Format Patent
LanguageEnglish
Japanese
Published 10.10.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a method for efficiently producing a fibrous carbon nano structure dispersion excellent in long-term stability while preventing the occurrence of bubbling during dispersion treatment.SOLUTION: A method for producing a fibrous carbon nano structure dispersion includes a step of subjecting a composition containing a fibrous carbon nano structure and a solvent to dispersion treatment. When a content of a dispersant in the composition is 0 pt.mass or more and less than 60 pts.mass based on 100 pts.mass of the fibrous carbon nano structure, and the dispersion treatment is conducted by using a medialess disperser 1 including a stator 3 and a rotor 2, a product S×W of a peripheral velocity S (m/s) of the rotor 2 and a ratio W of a maximum value W1 (m) of a width of a slit 4 to a minimum value W2 (m) thereof, during the dispersion treatment, is 10-200.SELECTED DRAWING: Figure 1 【課題】分散処理の際の泡立ちを抑制しつつ、長期安定性に優れる繊維状炭素ナノ構造体分散液の効率的製造方法の提供。【解決手段】繊維状炭素ナノ構造体と、溶媒とを含有する組成物に分散処理を施す工程を含む、繊維状炭素ナノ構造体分散液の製造方法であって、組成物中の分散剤の含有量を繊維状炭素ナノ構造体100質量部当たり0質量部以上60質量部未満とし、分散処理を、ステーター3とローター2を備えるメディアレス分散機1を用いて行い、分散処理の際のローター2の周速S(m/s)と、スリット4の幅の最小値W2(m)に対する最大値W1(m)の比Wとの積S×Wの値が、10以上200以下である製造方法。【選択図】図1
Bibliography:Application Number: JP20180060432