POLYESTER RESIN COMPOSITION FOR REFLECTING MATERIAL, AND REFLECTING MATERIAL CONTAINING THE SAME

To provide a polyester resin composition for a reflecting material, capable of giving a reflecting material in which deterioration in reflectance due to exposure to heat and light is suppressed.SOLUTION: The polyester resin composition for a reflecting material contains 30 pts.mass or more and 80 pt...

Full description

Saved in:
Bibliographic Details
Main Authors TAKIZAWA NOBUHIRO, OGASAWARA HIDETO, KIDA MARIKO, MAEDA MASANOBU, TAKEHARA AKINOBU, MAKIGUCHI WATARU
Format Patent
LanguageEnglish
Japanese
Published 12.09.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide a polyester resin composition for a reflecting material, capable of giving a reflecting material in which deterioration in reflectance due to exposure to heat and light is suppressed.SOLUTION: The polyester resin composition for a reflecting material contains 30 pts.mass or more and 80 pts.mass or less of a polyester resin (A) having a melting point or a glass transition temperature of 250°C or higher, 0.1 pt.mass or more and 5.0 pts.mass or less of a modified olefin polymer (B) containing 0.2-1.8 mass% of a functional group structural unit containing a heteroatom, 0.1 pt.mass or more and 5.0 pts.mass or less of an unmodified olefin polymer (C), 5 pts.mass or more and 50 pts.mass or less of a white pigment (D), and 1 pt.mass or more and 50 pts.mass or less of an inorganic filler (E), provided that the total of (A)-(E) is 100 pts.mass.SELECTED DRAWING: None 【課題】本発明の課題は、熱や光への暴露による反射率の低下が抑制された反射材を付与しうる、反射材用ポリエステル樹脂組成物を提供することである。【解決手段】融点もしくはガラス転移温度が250℃以上であるポリエステル樹脂(A)30質量部以上80質量部以下と、ヘテロ原子を含む官能基構造単位を0.2〜1.8質量%含む変性オレフィン重合体(B)0.1質量部以上5.0質量部以下と、未変性オレフィン重合体(C)0.1質量部以上5.0質量部以下と、白色顔料(D)5質量部以上50質量部以下と、無機充填材(E)1質量部以上50質量部以下とを含み、ただし、成分(A)〜(E)の合計は100質量部である、反射材用ポリエステル樹脂組成物。【選択図】なし
Bibliography:Application Number: JP20180039685