OPTICAL FILM AND IMAGE DISPLAY UNIT

To provide an optical film that can improve yield during manufacture and scratch resistance, and an image display unit including the same.SOLUTION: According to one aspect of the present invention, there is provided an optical film 10 having a multilayer structure with two or more layers, where the...

Full description

Saved in:
Bibliographic Details
Main Authors OGAWA YOSHIMASA, EBISU KEISUKE, SATO JUN, KOSAKA YOSUKE, MATSUSHITA HIROKI
Format Patent
LanguageEnglish
Japanese
Published 08.08.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide an optical film that can improve yield during manufacture and scratch resistance, and an image display unit including the same.SOLUTION: According to one aspect of the present invention, there is provided an optical film 10 having a multilayer structure with two or more layers, where the surface resistance value on a surface 10A of the optical film 10 is 1×10Ω/square or less, and when a steel wool test is conducted in which the surface 10A of the optical film 10 is rubbed with steel wool back and forth 10 times at a speed of 50 mm/sec while a load of 1 kg/cmis applied to the steel wool, the absolute value of the difference between the haze value of the optical film 10 after the steel wool test and the haze value of the optical film 10 before the steel wool test is 0.1% or less.SELECTED DRAWING: Figure 1 【課題】製造時の歩留まりおよび耐擦傷性を向上させることが可能な光学フィルムおよびこれを備えた画像表示装置を提供する。【解決手段】本発明の一の態様によれば、2層以上の多層構造を有する光学フィルム10であって、光学フィルム10の表面10Aにおける表面抵抗値が、1×1014Ω/□以下であり、光学フィルム10の表面10Aに対しスチールウールに1kg/cm2の荷重を加えながら、速度50mm/秒で10往復擦るスチールウール試験を行ったとき、スチールウール試験後の光学フィルム10のヘイズ値とスチールウール試験前の光学フィルム10のヘイズ値との差の絶対値が0.1%以下である、光学フィルム10が提供される。【選択図】図1
Bibliography:Application Number: JP20180013597