ETHYLENE/TETRAFLUOROETHYLENE COPOLYMER
To provide an ethylene/tetrafluoroethylene copolymer excellent in heat stability, and capable of reducing coloring.SOLUTION: In an ethylene/tetrafluoroethylene copolymer, a thermal decomposition start temperature is 370°C or higher, a yellow index value is -40 or lower, and a yellow index change deg...
Saved in:
Main Authors | , , , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
13.06.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | To provide an ethylene/tetrafluoroethylene copolymer excellent in heat stability, and capable of reducing coloring.SOLUTION: In an ethylene/tetrafluoroethylene copolymer, a thermal decomposition start temperature is 370°C or higher, a yellow index value is -40 or lower, and a yellow index change degree after being heated at 232°C for 168 hours is 100 or lower. In the ethylene/tetrafluoroethylene copolymer, a mol ratio (a)/(b) between a polymerization unit (a) based on ethylene and a polymerization unit (b) based on tetrafluoroethylene is 50-10/50-90.SELECTED DRAWING: None
【課題】熱安定性に優れ、着色を低減できるエチレン/テトラフルオロエチレン共重合体を提供する。【解決手段】熱分解開始温度が370℃以上であり、かつ、イエローインデックス値が−40以下であり、232℃で168時間加熱後のイエローインデックス変化度が100以下であるエチレン/テトラフルオロエチレン共重合体。エチレンに基づく重合単位(a)とテトラフルオロエチレンに基づく重合単位(b)とのモル比(a)/(b)が50〜10/50〜90であるエチレン/テトラフルオロエチレン共重合体。【選択図】なし |
---|---|
Bibliography: | Application Number: JP20170217774 |