MOISTURE-ABSORPTIVE ACRYLONITRILE-BASED FIBER, PRODUCTION METHOD OF THE FIBER, AND FIBER STRUCTURE CONTAINING THE FIBER

To provide an acrylonitrile-based fiber which can be continuously produced by a method simpler than conventional methods, is almost free from redness, and has high moisture absorptivity.SOLUTION: The moisture-absorptive acrylonitrile-based fiber comprises a polymer which is substantially free from c...

Full description

Saved in:
Bibliographic Details
Main Authors KOMIYAMA TAKUZO, MIZUTANI KENTA
Format Patent
LanguageEnglish
Japanese
Published 18.04.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:To provide an acrylonitrile-based fiber which can be continuously produced by a method simpler than conventional methods, is almost free from redness, and has high moisture absorptivity.SOLUTION: The moisture-absorptive acrylonitrile-based fiber comprises a polymer which is substantially free from crosslinked structures derived from covalent bonds, wherein the moisture-absorptive acrylonitrile-based fiber has a carboxyl group amount of 0.2-4.5 mmol/g, saturated moisture absorptivity at 20°C and 65%RH of 5 wt.% or higher, and water swelling degree of 10-folds or under.SELECTED DRAWING: None 【課題】従来、アクリル繊維に吸湿性を付与した繊維は知られているが、製造工程が多く生産性が低いものであったり、あるいは赤みを抑制しつつ吸湿性を高めることが難しいものであったりした。本発明は、かかる従来技術の現状に鑑みて創案されたものであり、その目的は、従来より簡便な工程で連続生産することができ、赤みがほとんどなく、高い吸湿性を有するアクリロニトリル系繊維を提供することにある。【解決手段】共有結合による架橋構造を実質的に有さない重合体で構成されている吸湿性アクリロニトリル系繊維であって、繊維中のカルボキシル基量が0.2〜4.5mmol/gであること、及び繊維の20℃×65%RHでの飽和吸湿率が5重量%以上であり、かつ水膨潤度が10倍以下であることを特徴とする吸湿性アクリロニトリル系繊維。【選択図】なし
Bibliography:Application Number: JP20180172009