Summary:To provide service-run parts with a great mechanical strength with a controlled narrow brazing gap size.SOLUTION: A method comprises the steps of: machining a tapered slot in a component 101; measuring the tapered slot to determine the dimensions 102; forming an insert to have a geometry corresponding to the tapered slot with a braze gap between an outer surface of the insert and an inner surface of the tapered slot 103; depositing a layer of a braze material on the outer surface of the insert 104, where the thickness of the layer corresponds to the braze gap; sintering the layer of the braze material on the outer surface of the insert to fabricate a diffusion layer 105; positioning the insert in the tapered slot 106; and brazing the diffusion layer to join the insert to the tapered slot 107. The treated component includes a surface having a tapered slot, an insert, and a braze joint.SELECTED DRAWING: Figure 1 【課題】ロウ付けギャップサイズを小さく制御することによりサービスランパーツに高い機械強度を与える。【解決手段】部品にテーパ付きスロットを機械加工し101、テーパ付きスロットは、寸法を決定するために計測される102。インサートが、インサートの外面とテーパ付きスロットの内面との間のロウ付けギャップを伴って、テーパ付きスロットに対応する幾何形状を有するように形成される103。ロウ付け材料の層がインサートの外面に付着され104、層の厚さがロウ付けギャップに対応する。インサートの外面にあるロウ付け材料の層は、拡散層を形成するように焼結される105。インサートは、テーパ付きスロット内に配置される106。拡散層は、インサートをテーパ付きスロットに結合するようにロウ付けされる107。処理された部品は、テーパ付きスロットを有する表面、インサート、およびロウ付けジョイントを含む。【選択図】図1
Bibliography:Application Number: JP20170245718