NON-ORIENTED ELECTROMAGNETIC STEEL SHEET
PROBLEM TO BE SOLVED: To provide a non-oriented electromagnetic steel sheet achieving both of improvement of die stamping accuracy and low iron loss, and a manufacturing method therefor.SOLUTION: There is adopted a non-oriented electromagnetic steel sheet containing, by mass%, C:0.0030% or less, Si:...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
04.10.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a non-oriented electromagnetic steel sheet achieving both of improvement of die stamping accuracy and low iron loss, and a manufacturing method therefor.SOLUTION: There is adopted a non-oriented electromagnetic steel sheet containing, by mass%, C:0.0030% or less, Si:2.0% to 4.0%, Al:0.1% to 3.0%, Mn:0.10% to 2.00%, P:0.09% or less, S:0.0050% or less, N:0.0050% or less, and the balance Fe with 0 impurity element, and having surface covering of an internal oxidation layer of a surface of 10 to 70% of all surface area and average internal oxidation layer thickness of an area where the internal oxidation layer exists of 0.5 μm to 10 μm.SELECTED DRAWING: None
【課題】打ち抜き精度の向上と低鉄損を両立する無方向性電磁鋼板、及びその製造方法を提供する。【解決手段】質量%で、C:0.0030%以下、Si:2.0%以上4.0%以下、Al:0.1%以上3.0%以下、Mn:0.10%以上2.00%以下、P:0.09%以下、S:0.0050%以下、N:0.0050%以下を含有し、残部Feおよび0不純物元素よりなり、表面の内部酸化層が覆う表面積が全表面積の10〜70%であり、内部酸化層のある領域の平均内部酸化層厚が0.5μm〜10μmであることを特徴とする無方向性電磁鋼板を採用する。【選択図】なし |
---|---|
Bibliography: | Application Number: JP20170050085 |