COMPONENT AND MANUFACTURING METHOD THEREOF
PROBLEM TO BE SOLVED: To provide: a component with little heat treatment strain and excellent abrasion resistance and fatigue characteristics; and a manufacturing method thereof.SOLUTION: The component has a constituent composition comprising prescribed constituents with a Z value of 30 or more defi...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
13.09.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide: a component with little heat treatment strain and excellent abrasion resistance and fatigue characteristics; and a manufacturing method thereof.SOLUTION: The component has a constituent composition comprising prescribed constituents with a Z value of 30 or more defined by formula (1), namely, Z=186-449C+38Si-8Mn-4Ni+7Cu-29Cr+15Mo+165V+142Ti-252Nb+368Al+4210B. The constitution to the depth of 100 μm from a surface of the component contains retained austenite of a volume fraction of 30% or less with the balance consisting of one or both of martensite and bainite. The constitution other than the nitrided part contains ferrite of an area fraction of 5-60%, and one or both of martensite and bainite of a total area fraction of 40-95%.SELECTED DRAWING: None
【課題】熱処理歪が少なく、かつ耐摩耗性と疲労特性に優れた部品およびその製造方法を提供する。【解決手段】所定の成分からなり、かつ、下記(1)式で定義されるZ値が30以上である成分組成を有し、前記部品の表面から100μmの深さまでの組織が、残留オーステナイトの体積率が30%以下であり、残部がマルテンサイトおよびベイナイトの一方または両方からなり、前記浸窒部以外における組織が、フェライトを面積率で5〜60%、マルテンサイトおよびベイナイトの一方または両方を合計面積率で40〜95%含む、部品。Z=186−449C+38Si−8Mn−4Ni+7Cu−29Cr+15Mo+165V+142Ti−252Nb+368Al+4210B ・・・(1)【選択図】 なし |
---|---|
Bibliography: | Application Number: JP20170037567 |