ALL-SOLID BATTERY

PROBLEM TO BE SOLVED: To provide an all-solid battery which is small in environmental load, and which can achieve both of a high adhesion strength and superior battery characteristics.SOLUTION: An all-solid battery 100 comprises: a positive electrode layer 20 having a positive electrode current coll...

Full description

Saved in:
Bibliographic Details
Main Authors HASEGAWA KENTA, KUROMIYA TAKAO
Format Patent
LanguageEnglish
Japanese
Published 09.08.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide an all-solid battery which is small in environmental load, and which can achieve both of a high adhesion strength and superior battery characteristics.SOLUTION: An all-solid battery 100 comprises: a positive electrode layer 20 having a positive electrode current collector 6, and a positive electrode mixture layer 21 formed on the positive electrode current collector 6 and including at least a positive electrode active material 2 and a binder 4; a negative electrode layer 30 having a negative electrode current collector 7, and a negative electrode mixture layer 31 formed on the negative electrode current collector 7 and including at least a negative electrode active material 3 and a binder 4; and a solid electrolyte layer 40 disposed between the positive electrode mixture layer 21 and the negative electrode mixture layer 31 and including at least a solid electrolyte 1 having ion conductivity. The concentration of solvent included in at least one layer selected from a group consisting of the positive electrode mixture layer 21, the negative electrode mixture layer 31 and the solid electrolyte layer 40 is 50 ppm or less. The concentration of the binder 4 included in at least one layer selected from the positive electrode mixture layer 21 and the negative electrode mixture layer 31 in the vicinity of the solid electrolyte layer 40 is lower than that in the vicinity of the positive electrode current collector 6 or the negative electrode current collector 7.SELECTED DRAWING: Figure 1 【課題】環境負荷が小さく、かつ高い密着強度と優れた電池特性とを両立する全固体電池を提供する。【解決手段】全固体電池100は、正極集電体6と、正極集電体6上に形成された、少なくとも正極活物質2およびバインダー4を含む正極合剤層21とを備える正極層20と、負極集電体7と、負極集電体7上に形成された、少なくとも負極活物質3およびバインダー4を含む負極合剤層31とを備える負極層30と、正極合剤層21と負極合剤層31との間に配置された、少なくともイオン伝導性を有する固体電解質1を含む固体電解質層10と、を備え、正極合剤層21、負極合剤層31および固体電解質層40よりなる群から選ばれた少なくとも一層に含まれる溶剤の濃度が50ppm以下であり、正極合剤層21および負極合剤層31から選ばれた少なくとも一層に含まれるバインダー4の濃度が、固体電解質層40近傍よりも正極集電体6又は負極集電体7近傍の方が高い。【選択図】図1
Bibliography:Application Number: JP20170018891